Hello all. New to the forum...but have been doing carbon work and fiberglassing for quite some time. Having some issues with my carbon fiber emblems. I am using a vac bag set up with a couple fiberglass molds I made. They have a super smooth orange gel coat and have release wax and pva. Everything looks great at first but No matter what,  can't get these things to come out right. Any ideas?

http://www.talkcomposites.com/Uploads/Images/2edd0228-ca44-4533-aab6-7586.JPG


Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Looks like it's bridging to me?