Reuseable silicone vacuum bags


Author
Message
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Well guys, I would really like to see you make a video on the ins and outs of reusable silicone vacuum bags.
I sense that for making many simple parts this is the way to go. Painfully little on the web on how to make them.
I have looked at all of the Smooth-on videos. They leave out how you would infuse carbon fiber cloth or twill. They do infuse chop matt without a flow media. How would you do carbon fiber twill? Have any of you other guys had any professional experience using this method for high volumes of parts?
Thanks
Fred    
Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
have a look on alan harpers website plenty of information there. Im still hoping to purchase one through work for our medium to large moulds.
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Thanks for the connection. I still need more how to than that site provided.
Can you use silicone bags to infuse carbon fiber twill. I have only seen infusion of glass matte.
Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search