XCR Skinning process


Author
Message
Lenny
Lenny
Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)Supreme Being (259 reputation)
Group: Forum Members
Posts: 16, Visits: 58
I would like to carbon skin a part and I have a question regarding the 'tack' time before applying the carbon.  The part I want to skin is quite large and has complex surfaces.  I don't want the resin base coat to be really tacky as once you lay the carbon it is very difficult to manipulate into position within damaging the weave pattern.   Therefore, could you lay the carbon earlier, so that the base coat is not so tacky and allows you to manipulate the carbon ? The process states 1-2 hours, but laying on after 10-30 minutes, would this cause any issues ?
Reply
Davidcorrado
Davidcorrado
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 5, Visits: 35
Hello EasyComposite Team 

how many basecoat/coating resin,i will  use 

element dimensions 6cmx27cm 

carbon fiber fabric  2x2 twill 3k 240g 

sorry for my english.

Regards
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lenny - 10 Years Ago
matthieutje65 - 10 Years Ago
Warren (Staff) - 10 Years Ago
Matt (Staff) - 10 Years Ago
67redrocket - 10 Years Ago
Dravis - 10 Years Ago
Lenny - 10 Years Ago
Warren (Staff) - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Warren (Staff) - 10 Years Ago
JonS - 10 Years Ago
Dravis - 10 Years Ago
Dravis - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
meir - 10 Years Ago
Davidcorrado - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Davidcorrado - 10 Years Ago
Warren (Staff) - 10 Years Ago
Umut Can Kizilray - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search