Group: Forum Members
Posts: 29,
Visits: 154
|
Hey guy's so I finally finished sanding all of my pieces that I overlay-ed with carbon fibre. I was told to sand all the way to 1200 Grit. The reason I chose to clear coat instead of polish, is the fact that my parts will be in direct sunlight for most of the time, and From what I read in the epoxy I used, there is not to much UV protection. Wondering what is the best clear coat to use for this?
|