Hey guy's so I finally finished sanding all of my pieces that I overlay-ed with carbon fibre. I was told to sand all the way to 1200 Grit. The reason I chose to clear coat instead of polish, is the fact that my parts will be in direct sunlight for most of the time, and From what I read in the epoxy I used, there is not to much UV protection. Wondering what is the best clear coat to use for this? 
Reply
Superleggera
Superleggera
Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)
Group: Forum Members
Posts: 15, Visits: 399
Do you plan on spraying yourself or taking your parts to a painter?