i was wondering the same thing.
doing some research, i see many that recommends this two parts clear.
https://www.amazon.com/gp/product/B0043B7UQY/ref=oh_aui_detailpage_o02_s00?ie=UTF8&psc=1
i ordered a can for experimenting, and hope to get good results.
will report as soon as i have some (results that is BigGrin)
2 things to take in consideration.
1. being 2 parts clear, it is more toxic than the 1 part, so you will need to use proper protection.
2. the can is good for 12 hours once the two parts are mixed, so it's better to clear multiple projects at the same time.
as i'm doing my first steps with car part skinning, i'm trying to decide if to clear coat or just buff the epoxy.
i got the XCR resin so it should have some UV protection qualities. not sure to what level.
not to hijack this thread, i will open a separate on on the subject.
Superleggera
Superleggera
Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)
Group: Forum Members
Posts: 15, Visits: 399
Do you plan on spraying yourself or taking your parts to a painter?
deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Hey guy's so I finally finished sanding all of my pieces that I overlay-ed with carbon fibre. I was told to sand all the way to 1200 Grit. The reason I chose to clear coat instead of polish, is the fact that my parts will be in direct sunlight for most of the time, and From what I read in the epoxy I used, there is not to much UV protection. Wondering what is the best clear coat to use for this? 