Looking to get into infusion.. really would like to buy a whole kit with pump I would like to get a pump I can grow into and not have to replace it as my skills grow. Looking for suggestions. 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Just get the Easy Composites infusion starter kit? 
TheRacer02
TheRacer02
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 48
I would rather not ship from UK to us shipping would cost as much as a pump alone I would imagine 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
where are you located?

a decent vac pump is your main equipment and of course all the consumables, like bagging filmand infusion mesh
TheRacer02
TheRacer02
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 48
I am located in phx az. I have been looking at a few online just haven't pulled the trigger on any yet
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
http://www.ebay.com/itm/1-0-Gal-SS-Vacuum-Chamber-3-0-CFM-Vacuum-Pump-Kit-With-SlickVacSeal-/111845057070?hash=item1a0a7c222e:g:rykAAOSwKfVXIlDG

this looks like a good buy to get you started, i looked in the aircraft spruce catalogue but it was a lot more expensive for just a pump