ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
http://www.ebay.com/itm/1-0-Gal-SS-Vacuum-Chamber-3-0-CFM-Vacuum-Pump-Kit-With-SlickVacSeal-/111845057070?hash=item1a0a7c222e:g:rykAAOSwKfVXIlDG
this looks like a good buy to get you started, i looked in the aircraft spruce catalogue but it was a lot more expensive for just a pump
Reply
Like
2
TheRacer02
TheRacer02
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 48
I am located in phx az. I have been looking at a few online just haven't pulled the trigger on any yet
Reply
Like
3
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
where are you located?
a decent vac pump is your main equipment and of course all the consumables, like bagging filmand infusion mesh
Reply
Like
2
TheRacer02
TheRacer02
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 48
I would rather not ship from UK to us shipping would cost as much as a pump alone I would imagine
Reply
Like
3
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Just get the Easy Composites infusion starter kit?
Reply
Like
3
TheRacer02
TheRacer02
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 48
Looking to get into infusion.. really would like to buy a whole kit with pump I would like to get a pump I can grow into and not have to replace it as my skills grow. Looking for suggestions.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search