Embossing C.F


Author
Message
Coaly
Coaly
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 4, Visits: 30
Hey again,

Do you think its possible to emboss or etch carbon fibre. Like a Logo.

The only disadvantage I can think of would be if its too deep, it may break the fibre and melt the resin around the surroundings.
Edited 13 Years Ago by Coaly
Replies
CarbonMike
CarbonMike
Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)
Group: Forum Members
Posts: 31, Visits: 45
You can shot blast it using a fine glass media, the same way companies etch glass. Also gives an awesome key for spraying a clear coat laquer onto it leaving no visible evidence of any kind media blasting but improves the gloss ten fold!
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Carbon Mike

Could you post a few pictures of parts you have done this technic to?

I did something similar years ago where I got a cut out label taped down to polished stainless steel and lightly sand blasted it.

It came out really nice. I am curious what it looks like on Carbon Fiber.

Thanks

Fred  
CarbonMike
CarbonMike
Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)
Group: Forum Members
Posts: 31, Visits: 45
How do. Yeah I can fire some pics up but not for a few days as I'm away from home at the minute on my Christmas holidays at the inlays lol