Hey again,

Do you think its possible to emboss or etch carbon fibre. Like a Logo.

The only disadvantage I can think of would be if its too deep, it may break the fibre and melt the resin around the surroundings.
By CarbonMike - 12/28/2012 12:21:40 PM

Warren (27/12/2012)
Sounds like an interesting technique!!


Lol it's not really as interesting as it sounds but it works very well. It's the same method you'd use if you we're bonding two carbon parts together, basically you'd just be giving the surface a good key.