SUPERTIA
SUPERTIA
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 65
Hi guys, this is my first post.. i used the search button, but i haven't found my answer. When i demold my pieces in 70% of cases i have this problem, air on surface. I do this pieces for cosmetically use, so i'm expect them are perfect.. Can u help me? Here pics of the result
Reply
Like
2
Reply
SUPERTIA
SUPERTIA
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 8,
Visits: 65
[Quote] [b] Hanaldo (30/05/2016) [/ b]
Yeh ho intuito che era il problema.
L'infusione deve essere stretto assolutamente al 100%.
Si dovrebbe essere in grado di tornare alla parte una settimana dopo l'infusione e ancora trovare la stretta borsa.
[/citazione]
Tomorrow evening i'll try to leave the vaccum for more than 15m, it might the pump (electric, like EC site) has little air losses?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
surface problem
SUPERTIA
-
9 Years Ago
Are you wet laying or infusing? Either way, not enough resin and too much air are your problem.
Hanaldo
-
9 Years Ago
thanks for the answer hanaldo! I work with the infusion system, i do the vacuum, and wait around...
SUPERTIA
-
9 Years Ago
if you are after a good finish for cosmetics then hold back on the infusion and wait longer before...
VVS
-
9 Years Ago
[Quote] [b] VVS (30/05/2016) [/ b] [hr] se siete dopo una buona finitura per la cosmesi poi...
SUPERTIA
-
9 Years Ago
Yeh I guessed that was the problem. Infusion needs to be absolutely 100% tight. You should be able...
Hanaldo
-
9 Years Ago
[Quote] [b] Hanaldo (30/05/2016) [/ b] [hr] Yeh ho intuito che era il problema. L'infusione deve...
SUPERTIA
-
9 Years Ago
Leave the vacuum for at least half an hour, preferably one hour. You should clamp the part off from...
Hanaldo
-
9 Years Ago
here we are ... I decided to change some working methods .. first of all, put everything in a bag...
SUPERTIA
-
9 Years Ago
Don't worry if it is flowing quickly as this will not affect the part, I only say slow it down by...
VVS
-
9 Years Ago
A friend told me that my infusion mesh is not good, but i think the only problem i have is about air...
SUPERTIA
-
9 Years Ago
Nah. Flow mesh can either work, or not work. If your mesh doesn't work, then your part simply won't...
Hanaldo
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search