Hi guys, this is my first post.. i used the search button, but i haven't found my answer. When i demold my pieces in 70% of cases i have this problem, air on surface. I do this pieces for cosmetically use, so i'm expect them are perfect.. Can u help me? Here pics of the result
By Hanaldo
-
6/4/2016 3:11:22 AM
Nah. Flow mesh can either work, or not work. If your mesh doesn't work, then your part simply won't infuse, it won't cause issues like this.
This is 100% an air leak issue.