As the title says,going to be making a 2 piece mould of a GSXR 1000
tailpiece,and I'm having trouble getting my head round it.The top is OK
it the underneath that's the problem,as you can see in the picture it
has a lip,so would the flange be best at 90 degrees or straight,as I
will be vacuum bagging the part when I make it,how do I hold the carbon
inplace.Hope I've made myself clear,in my head I know what I want to
say,but when it comes to writing it down it goes out the window.Crazy
Any advise is appreciated.

   Thanks Paul

http://www.talkcomposites.com/Uploads/Images/0657d2ba-08b7-4811-80d6-010d.jpghttp://www.talkcomposites.com/Uploads/Images/0aa7103c-48e2-4bdc-8a43-652f.jpghttp://www.talkcomposites.com/Uploads/Images/0b407754-07fd-49f1-9c9f-681a.jpg
Reply
Paul M
Paul M
Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)Supreme Being (142 reputation)
Group: Forum Members
Posts: 18, Visits: 79
Cheers for the reply,will be infusion,think it will be 90 deg flanges.