Finishing Epoxy coat


Author
Message
franckG31
franckG31
Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)Forum Member (41 reputation)
Group: Forum Members
Posts: 3, Visits: 8
When I apply Clear Epoxy on top of the parts I make, it often runs of from some areas ?

Any idea on how to prevent that ?

I tried degreasing the part with alcool, it was worst than ever.
Reply
FalleN
FalleN
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 74
So I should scuff the previous epoxy layer up with 80 grit before applying a new layer? Seems to rough to me, but I'll test it.
I hope it won't affect the physical appearance of the parts, since these are for show on a car.

Thanks for the response Smile