4/3/2015 7:01:38 PM
When I apply Clear Epoxy on top of the parts I make, it often runs of from some areas ?
Any idea on how to prevent that ?
I tried degreasing the part with alcool, it was worst than ever.
By FalleN
-
4/7/2016 3:27:31 PM
So I should scuff the previous epoxy layer up with 80 grit before applying a new layer? Seems to rough to me, but I'll test it.
I hope it won't affect the physical appearance of the parts, since these are for show on a car.