Use a "coating epoxy" that has some thickening agent in it, to prevent it from sagging and running off.
Also paint on a very thin layer then wait until it is almost hard, but still a bit "tacky" in the surface, then paint another thin layer .. keep going until you have the desired thickness..
If you leave the thin layer to cure fully, then you must wet-sand the surface carefully before applying the next coat.