In 123.jpg file.
1. Gauge the correct amount of resin
The amount of resin that your project will need will vary upon its size and the amount of reinforcement you have
used; more layers of reinforcement will be able to support more resin.
Use the table below to calculate approximately how much resin your finished part will use (see the PART column), and
how much you should mix (see the MIX column) to ensure you have enough project will require:
see the 234.jpg

so we can calculate the resin weight content is 80/(200+80)=28.5%, This is very very low.
Is it right? OR we often beliven the resin weight is 40%?

beijing of China
Attachments
123.jpg (1.8K views, 149.00 KB)
234.jpg (1.7K views, 126.00 KB)
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
I just weigh everything (mesh included), use that amount of resin then and add a bit for the tubes and pot