Hi I am doing Vacuum Bagging and in the final part there are gaps/voids where the warp and wept intersect. Here is an image of it. Can anyone help please?
Attachments
IMG_20160224_221923626_HDR.jpg (2.4K views, 1.00 MB)
Reply
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Not enough consolidation + resin starved (severely!) --   Vacuum leak or not enough vacuum?  Not enough resin (Wet-lay with Vac-bagging?)

To give you really useful advice we need complete info on materials used and process/technique --

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search