Vacuum Bagging - Problem with surface finish


Author
Message
Ashutosh
Ashutosh
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 28
Hi I am doing Vacuum Bagging and in the final part there are gaps/voids where the warp and wept intersect. Here is an image of it. Can anyone help please?
Attachments
IMG_20160224_221923626_HDR.jpg (2.2K views, 1.00 MB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Are you not using a perforated release film between the peel ply and the breather? 