Has anyone had any practical experience thinning epoxy resin for infusion ?

I have been advised that if I use MEK at no more than 2% in the part A  it will be ok.

I understand that there may be a reduction in strength which wont be an issue for the parts I make.



Reply
rallyfly
rallyfly
Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)
Group: Forum Members
Posts: 25, Visits: 85
They tell me its  600 mPas @25 C