Can a mirror be used instead of e.g. glass to get a good finish or will it be a problem with the epoxy?
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I have infused a lot of smaller pieces of CF on an old mirror, glued ( with epoxy .. ) on top of a thick piece of plywood ..  Works fine ..

A sheet of thick plate glass is better, for the simple reason that you can check your infusion from the "finish side" through the glass ..

I mainly use "EC Easy-lease" on the glass ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search