Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I have infused a lot of smaller pieces of CF on an old mirror, glued ( with epoxy .. ) on top of a thick piece of plywood .. Works fine ..
A sheet of thick plate glass is better, for the simple reason that you can check your infusion from the "finish side" through the glass ..
I mainly use "EC Easy-lease" on the glass ..