Dear all,

When using the pump, some oïl began to rise up in the connector of the pump. We have no clue of the origin of the problem, so maybe one of you has already been facing this matter and knows how to prevent it? We do not plan to use again the pump since the problem is not solved.

For information, the level of oïl dramatically decreased but there was still the minimum content needed for good use.

Thanks in advance for your answer.

Karine
Reply
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Hello Karine,

This is a fairly simple one to solve. Before turning off the pump, you should always ensure that you close the quarter turn valve (fitted to the pump itself) - Otherwise the level of vacuum in the lines/bag will draw the oil out of the pump and towards the catchpot. By closing the valve, there is no way for the oil to draw up the lines.

Let us know if you have any further problems.