By Karine63 - 1/15/2016 11:36:07 AM
Dear all,
When using the pump, some oïl began to rise up in the connector of the pump. We have no clue of the origin of the problem, so maybe one of you has already been facing this matter and knows how to prevent it? We do not plan to use again the pump since the problem is not solved.
For information, the level of oïl dramatically decreased but there was still the minimum content needed for good use.
Thanks in advance for your answer.
Karine
|
By Karine63 - 1/16/2016 9:03:27 AM
Thanks a lot for your answers and your advice! The oil no longer rose during infusion. I did the mistake once, I will remember it for the next times!
|
|