Group: Forum Members
Posts: 11,
Visits: 167
|
Hi, my first mould is of a money tray that I borrowed from the local harvester, first lost vacuum during and second lost vac about 45 mins after I infused it because I decided to move it and the feed in line leaked. Both have actually turned out ok but its all good as I am learning a lot. I will be doing another this morning as soon as I have cleaned the mould.
First big project will be body panels for race cars and various supercars, most will be painted but I want to get the finish perfect on every single one.
Nothing good to say......then say nothing
|