By LeeBrett - 1/8/2016 10:41:01 AM
Hi, been viewing this forum for a week or so and have now decided to take the step and start making a few parts in carbon.
Looking at eventually making carbon panels for race cars and a few supercar panels for a company that I work for.
I have no experience at all so going to start with something small to mould and hopefully learn from my mistakes.
Looking forward to getting started and I am sure that I will be back on here soon to pick your brains when I make a mistake.
Lee Brett
|
By LeeBrett - 1/11/2016 9:17:38 AM
Hi, my first mould is of a money tray that I borrowed from the local harvester, first lost vacuum during and second lost vac about 45 mins after I infused it because I decided to move it and the feed in line leaked. Both have actually turned out ok but its all good as I am learning a lot. I will be doing another this morning as soon as I have cleaned the mould.
First big project will be body panels for race cars and various supercars, most will be painted but I want to get the finish perfect on every single one.
|
|