Zekewarg
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 42,
Visits: 241
Hi all!
Did a search but couldn't find any previous posts about it.
I'm looking for a high-temp resin that needs to be baked in an oven for cure, but I can't find any.
Anyone got a tip?
I want to be able to make a sort-of prepreg that will last för a while i a freezer, and even at room temp.
Also, where can I find completed vacuum-bags? I know I can make the with gumtape, but I would like purpose made bags with
zip-locks or similar. I've seen them being used on Youtube.
Thanks in advance.
Reply
Like
5
Reply
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
There's a plethora of resins available, but it's pretty hard to recommend something without knowing your area...
As for the zip-lock vacuum bags, I presume you are talking about these:
They are storage bags for vacuum packing things like clothing and bedding. Most home department stores will sell them in various sizes, otherwise you can get them on eBay.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Where to find High-Temp resin and vacuum-bags?
Zekewarg
-
10 Years Ago
There's a plethora of resins available, but it's pretty hard to recommend something without knowing...
Hanaldo
-
10 Years Ago
I need a resin for automotive parts. Roofrack, crates, boxes, air intakes and such.
Zekewarg
-
10 Years Ago
Apologies, I meant area as in location. Are you in the UK?
Hanaldo
-
10 Years Ago
Ah, my bad. No I live in Sweden. I usually buy from EC but they don't seem to carry bake-resin.
Zekewarg
-
10 Years Ago
Is the EC high temp resin not sufficient? So you want something that won't have an initial cure at...
Hanaldo
-
10 Years Ago
Precisely! I want to be able to prep a fair amount and store it in sub0 temps. But I can't find any...
Zekewarg
-
10 Years Ago
Hysol stuff is top shelf, it's made for aerospace application so sold to Boeing etc.
Hanaldo
-
10 Years Ago
Seriously, I have now searched for several days and I can find absolutely nothing. Temp-cured epoxy...
Zekewarg
-
10 Years Ago
http://www.axson-technologies.com/en/find-product/Laminating-Products/Epoxy-laminating-systems
Fasta
-
10 Years Ago
I checked the site, couldn't work out which ones where temp-curing? Perhaps the EC staff could...
Zekewarg
-
10 Years Ago
Our Very High Temperature Epoxy resin WILL cure at room temperature so is NOT really suitable for...
Warren (Staff)
-
10 Years Ago
maybe http://www.fibermaxcomposites.com/shop/epoxy-systembrr244-h33-p-100213.html?cPath=26
tomzi1234
-
10 Years Ago
YES! Thank you! Will try them and perform some stresstesting. Thanks again!
Zekewarg
-
10 Years Ago
RE the prepreg: I'm not following what you want, just pick a high temp prepreg that has a 7+ day...
ChrisR
-
10 Years Ago
If I get it right you need HT resin for making molds. I would recommend you Axson Epolam 2031.I...
Keko
-
10 Years Ago
Gurit or gruit one of the two I think or maybe alchemie they don't do prices online you gotta...
Davidpetty1988
-
9 Years Ago
Why do you need or want to make your own pre preg? The stuff you can buy ready to go is all great,...
Fasta
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search