By Zekewarg
-
10/29/2015 12:06:39 PM
Hi all!
Did a search but couldn't find any previous posts about it.
I'm looking for a high-temp resin that needs to be baked in an oven for cure, but I can't find any.
Anyone got a tip?
I want to be able to make a sort-of prepreg that will last för a while i a freezer, and even at room temp.
Also, where can I find completed vacuum-bags? I know I can make the with gumtape, but I would like purpose made bags with
zip-locks or similar. I've seen them being used on Youtube.
Thanks in advance.
By Fasta
-
1/10/2016 2:07:37 AM
Why do you need or want to make your own pre preg?
The stuff you can buy ready to go is all great, the manufacturers of it have serious equipment for impregnating the fibre so that it has just the right amount of resin.