Hello I would make 3 suggestions. 1 make sure your mold is very warm 2 make sure your resin is very warm 3 Do not let the infusion front go at full speed or it may skip over parts as I see in your picture. open the feed line only enough to get the resin front moving at a slower feed which will allow the wetting process more time to fill every void. Hope this helps. Fred
|