How to joint carbon for hood
How to joint carbon for hood
Post Reply
Like
3
How to joint carbon for hood
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
rebew
rebew
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 172
Hello I have a problem I will make a bonnet which is 130 cm wide but my carbon fiber roll is only a meter wide How do I make a good looking joint? as on the picture
http://www1.garaget.org/gallery/archive/70842/large/731885_l7r7xo.jpg
Edited
10 Years Ago by
rebew
Reply
Like
3
Reply
Jacopo Carbonio
Jacopo Carbonio
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 43,
Visits: 109
You can lay a strip of scotch for the center line, after you lay the first carbon fabric following the line, you remove the scotch and you lay the second carbon fabric. I saw this technique several times.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How to joint carbon for hood
rebew
-
10 Years Ago
You can lay a strip of scotch for the center line, after you lay the first carbon fabric following...
Jacopo Carbonio
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search