Hello I have a problem I will make a bonnet which is 130 cm wide but my carbon fiber roll is only a meter wide How do I make a good looking joint? as on the picture
Jacopo Carbonio
Jacopo Carbonio
Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)Supreme Being (343 reputation)
Group: Forum Members
Posts: 43, Visits: 109
You can lay a strip of scotch for the center line, after you lay the first carbon fabric following the line, you remove the scotch and you lay the second carbon fabric. I saw this technique several times.