By rebew - 8/11/2015 10:40:47 AM

Hello I have a problem I will make a bonnet which is 130 cm wide but my carbon fiber roll is only a meter wide How do I make a good looking joint? as on the picture
By Jacopo Carbonio - 8/11/2015 11:42:36 AM