Beeing not as patient as i maybe should, i have just removed the mould.
Since i made it on a sheet of polypropylene which i also had waxed it came of witout any problems.
I made quite a mess, and see several things i could have done better, but i believe with some proper afterwork i can make it usable.
The gelcoat had found its way under on a couple of places, so i needed to cut the mould slightly


So next time ill make sure to be extra careful when adding the plasticine barrier.
Other than that the part came loose pretty easy without any damage.


So now its time for a lot of cutting and sanding before it is twaron infusion time.
Has anyone tried to infuse using the flexible resin? EF80