Group: Forum Members
Posts: 58,
Visits: 401
|
Thanks. Its actually a air deflector that leads the air out from the radiator, the engine is in the back =)
I have just added the coupling coat. I mixed 303g coupling gel and 5g of mekp on top in a plastic cup. What happened was that firstly within 5-8minutes the bottom of the cup had hardened, and second the cup started dissolving =). So i recon i need to use papercups and not plastic, but why did the gel harden so fast?
Didnt i mix the mekp rough enough maybe?
|