I found the tds sheet,they say you can partial post cure the system but i ask if someone know or ever try the partial cure,i want this info cause i need the higher tg at this post cure,i cannot raise the temp because i have the pastic cores under the carbon lamination,so i m looking to find if this high temp system can achieve a better tg after post curing at 70,than other usual laminating systems
|