Good afternoon to all,

I am building a female mold that will beused to make a carbon fibre marathon canoe (18’6”). I have good skills working with fibreglass but this is my first experience in making a femalemold.

The mold is based on wooden slats lined with 1” foam and  lined once more with fibreglass. The fibreglass  is then finished with the usual body fillerand mold primer/hi-gloss coats to make it a glass finish. As you may realise,the front and back end of the molds are extremely streamlined and I find itimpossible to sand down to a glass finish.

The alternatives that I have come up withwould be to 1) cut the mold in half and work on each side separately thenreassemble to lay the carbon fibre cloth. The disadvantage might be that Iwould not end up with symmetrical sides. Option 2 would be to lay the carbon fibrein the mold as is but finish the exterior of the canoe’s ends to a glass finishafterwards. Finishing the outside to a glass finish after unmolding seemsdifficult to achieve. Any comment and recommendation would be welcome. 

Manythanks.


Z


Replies
Zedok
Zedok
Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)Supreme Being (122 reputation)
Group: Forum Members
Posts: 18, Visits: 115
Many thanks Hanaldo and Dravis for your comments and encouragements. At least my observations are normal and I have not f***ed up... yet.
 
I have ordered a set of orbital 240, 400 and 800 orbital discs which should make the job easier. 

Spraying is not an option at this point. Anyhow, I would have to take time and learn how to spay correctly. Might as well take that time and sand. The idea of thinning the Gloss resin with 8% acetone seems very appealing and I shall have a try on a small part of the the pattern.

Hanaldo, you mentioned: "Fortunately, it's easy to fill these little holes and sand smooth. " Do you mean filling them with additional gloss resin? 

Cheers,
Z
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Zedok (29/06/2015)
Many thanks Hanaldo and Dravis for your comments and encouragements. At least my observations are normal and I have not f***ed up... yet.
 
I have ordered a set of orbital 240, 400 and 800 orbital discs which should make the job easier. 

Spraying is not an option at this point. Anyhow, I would have to take time and learn how to spay correctly. Might as well take that time and sand. The idea of thinning the Gloss resin with 8% acetone seems very appealing and I shall have a try on a small part of the the pattern.

Hanaldo, you mentioned: "Fortunately, it's easy to fill these little holes and sand smooth. " Do you mean filling them with additional gloss resin? 

Cheers,
Z


Yeh mate, just mix up a small amount of the gloss coat and and use a pop stick to dab it into the holes. Fill it proud of the surface so you can sand it down flat. Easy as. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Zedok - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
George Sychrovsky - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
George Sychrovsky - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
wozza - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 10 Years Ago
     Looking good :)
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago
VVS - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
VVS - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search