Good afternoon to all,

I am building a female mold that will beused to make a carbon fibre marathon canoe (18’6”). I have good skills working with fibreglass but this is my first experience in making a femalemold.

The mold is based on wooden slats lined with 1” foam and  lined once more with fibreglass. The fibreglass  is then finished with the usual body fillerand mold primer/hi-gloss coats to make it a glass finish. As you may realise,the front and back end of the molds are extremely streamlined and I find itimpossible to sand down to a glass finish.

The alternatives that I have come up withwould be to 1) cut the mold in half and work on each side separately thenreassemble to lay the carbon fibre cloth. The disadvantage might be that Iwould not end up with symmetrical sides. Option 2 would be to lay the carbon fibrein the mold as is but finish the exterior of the canoe’s ends to a glass finishafterwards. Finishing the outside to a glass finish after unmolding seemsdifficult to achieve. Any comment and recommendation would be welcome. 

Manythanks.


Z


Reply
George Sychrovsky
George Sychrovsky
Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)Supreme Being (228 reputation)
Group: Forum Members
Posts: 24, Visits: 1.6K
Now I see what you did there, this should be built as a "plug" first, nobody builds shapes like his directly into a female mold


---------------------------------------------------------------------
Disclaimer opinions of others will vary depending on what they are selling
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Zedok - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
George Sychrovsky - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
George Sychrovsky - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 11 Years Ago
wozza - 11 Years Ago
Dravis - 11 Years Ago
Zedok - 10 Years Ago
     Looking good :)
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago
VVS - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
VVS - 10 Years Ago
Zedok - 10 Years Ago
Zedok - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Dravis - 10 Years Ago
Zedok - 10 Years Ago
Hanaldo - 10 Years Ago

Similar Topics