BlackNDecker
BlackNDecker
Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Greetings all,

I bought a brand new OEM steel roof and plan to make a mold and eventually a carbon fiber roof. 

A little background...My car is a 2007 Honda Civic Si and comes with a heavy sun roof assembly (this comes standard from the factory). I contemplated simply swapping roofs for the OEM "non-sunroof" steel roof. That would save me around 20 lbs...but instead of going that direction I've decided to make a carbon fiber roof and hopefully save 30+ lbs.

Some pictures of my progress...

Made some progress on the roof project. 

Transferred it out to the garage:


The antenna hole will be covered:


And the tabs for the weather seal have to be cut off:


Luckily I have a Dremel for these types of projects:


Made some flanges:


Antenna hole covered (with a fresh coat of wax):


Flanged, waxed, and ready to go...




Unfortunately, it's going to be too humid all weekend to lay the gel coat...so I'll probably have to wait until Monday or Tuesday. fml
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely worth repairing, especially given it is a large flat surface. Will only take 20 minutes of sanding to get it perfect. 

I suggest doing the repairs sanding it flat and through to 1200, then give the whole mould a flat down with 1200 before compounding. You'll be amazed how much better the surface can be. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
BlackNDecker - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
BlackNDecker - 10 Years Ago
Jacopo Carbonio - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
BlackNDecker - 10 Years Ago
     Looking good.
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
Dravis - 10 Years Ago
BlackNDecker - 10 Years Ago
Jacopo Carbonio - 10 Years Ago
kidpaint - 10 Years Ago
BlackNDecker - 10 Years Ago
redeye - 10 Years Ago
BlackNDecker - 10 Years Ago
Warren (Staff) - 10 Years Ago
VVS - 10 Years Ago
BlackNDecker - 10 Years Ago
VVS - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
BlackNDecker - 10 Years Ago
Hanaldo - 10 Years Ago
davro - 10 Years Ago
BlackNDecker - 10 Years Ago
BlackNDecker - 10 Years Ago
Warren (Staff) - 10 Years Ago