kidpaint
kidpaint
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 99,
Visits: 676
I know that EC has an epoxy tooling gel coat, but for some reason when I search say google. I dont get any other hits of people selling it. Am I just naive and over looking something or whats the deal? Is an epoxy surface coat the same thing? I did search and still am unsure so sorry if this is a broken record question.
Reply
Like
2
redeye
redeye
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 559
I am in South Africa and have bought some epoxy tooling gelcoat there. In fact, finding polyester would have been more difficult (no issue as I wanted epoxy).
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Epoxy tooling gelcoat is certainly more specialist. I think you will find that not a lot of places will stock it, and even less will advertise it online. So you might be able to find it locally, but a google search might not be too revealing.
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Our
Epoxy Tooling Gel Coat
is specially formulated for us so you will not find one the same elsewhere. However there may well be some other resin companies formulating thier own epoxy tooling gelcoat, although as you are finding out, it is not a very common product in the industry.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
20_rc51_00
20_rc51_00
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
http://www.resinservices.com/custom.asp?CustomID=14
have used the alum filled epoxy in the past. Never at oven temps but it does claim good Tg and HDT's without any post cures.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search