6/11/2015 11:28:10 PM
I know that EC has an epoxy tooling gel coat, but for some reason when I search say google. I dont get any other hits of people selling it. Am I just naive and over looking something or whats the deal? Is an epoxy surface coat the same thing? I did search and still am unsure so sorry if this is a broken record question.
By 20_rc51_00
-
7/13/2015 8:03:34 PM
http://www.resinservices.com/custom.asp?CustomID=14
have used the alum filled epoxy in the past. Never at oven temps but it does claim good Tg and HDT's without any post cures.