Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Depending on the type of "canvas" it may work just fine .. It will add some strength, but not nearly as much as glass-fibre..
What you should have bought at the local hardware store is "Wall -glass mat" of the cheapest type without any primer or binder in ..
Works a treat with Epoxy ... and its cheap .. No idea how it would work with Polystyrene though- --