Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
KTM parts - mold making and advice please
KTM parts - mold making and advice please
Post Reply
Like
2
Prev
1
2
Jump To Page
KTM parts - mold making and advice please
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
redeye
redeye
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 559
Hey.
Welcome. What bike is it? Road going machine or dual sport, Enduro or MX? I have a KTM enduro bike (not that the brand is pertinent, I'm just showing off) and have been contemplating a variety of parts out of CF for it. I have however decided to leave plastics as they are for now as they are bound to take a beating if made in CF. I have however been thinking of some of the flexible resins, but have still considered plastics as on the back burner as I make other parts.
Reply
Like
3
simyboye
simyboye
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 45
Hi there,
New to the forum so good day to everyone.
I want to eventually convert all my plastics (fairings) to CF and having to wet lay as I will go to vacuum bagging at some point in the future.
I want to start with simple molds first but a few have flanges/ mounting points behind the plastics. What's the best way to do this? Been watching vids on here and pootube.
If I can upload an image will do so asap.
Until then many thanks.
Jay
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search