By simyboye - 5/18/2015 1:47:33 PM

Hi there,
New to the forum so good day to everyone.

I want to eventually convert all my plastics (fairings) to CF and having to wet lay as I will go to vacuum bagging at some point in the future.

I want to start with simple molds first but a few have flanges/ mounting points behind the plastics. What's the best way to do this? Been watching vids on here and pootube.

If I can upload an image will do so asap.

Until then many thanks.
Jay
By Jacopo Carbonio - 8/26/2015 11:34:58 PM

Hi! I found this page on FB and I follow him and his works, I was surprised byt his full carbon ktm..it's not so simple to make..