jt393
jt393
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 15
Good morning,
I'm wondering whether you have any information or data regarding the cell geometry of your honeycomb cores, both Nomex and Aluminium?
In particular, are they regular hexagons in shape (all sides the same length) and is the cell size measured from one flat side to the opposing flat side, rather than corder to corner or some other measurement?
Are there any variations in this in the Nomex and Aluminium you stock, or are they all the same?
Thanks for your help.
Reply
Like
18
Reply
jt393
jt393
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 15
That's really helpful to know in addition, thank you.
And I have found exactly the same with the Aluminium honeycomb, in terms of the expansion not creating the regular structure, though as you say it likely averages out over an area. I wonder whether we can find a way to expand the structure more repeatably than the DIY approaches using nails in wood and so on for simplicity. I'll let you know if I do.
I am especially interested in the machining side of things though, so it's great you've mentioned that. I too will be looking to machine down to 3mm and 5mm - could be a useful comparison with the Nomex. Do you have any tips or guidance as to how you found the machining to work best?
Thanks again, this is a great forum and though contacting EC directly was what I initially wanted to do, this is proving far more helpful and hopefully for future readers too.
Reply
Like
19
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Honeycomb Cell Geometry
jt393
-
11 Years Ago
Both nomex and aluminium honeycomb have similar cell shapes. The nomex uses bonded nomex paper, and...
Warren (Staff)
-
11 Years Ago
Thanks Warren, that is a really helpful response - the extra information especially. I am...
jt393
-
11 Years Ago
Yes that is correct, the cell size is d c in the picture.
Warren (Staff)
-
11 Years Ago
I can add that expanding the Alu honeycomb, and maintaining a regular hexagonal structure to the...
Dravis
-
11 Years Ago
That's really helpful to know in addition, thank you. And I have found exactly the same with the...
jt393
-
11 Years Ago
The expanding machines are a little bit more precise than the DIY method as the "fingers" on the...
Warren (Staff)
-
11 Years Ago
I've machined the alu honeycomb in unexpanded form. I made a "jig" to set up in my milling machine,...
Dravis
-
11 Years Ago
Several formulas about to machine crushed core to a profile then expand again have done repairs to...
f1rob
-
11 Years Ago
As for the "satellite" Aerospace jobs ... some of that is just mindblowing Tech.... :-O I've seen...
Dravis
-
11 Years Ago
Post Reply
Like
18
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search