Good morning,

I'm wondering whether you have any information or data regarding the cell geometry of your honeycomb cores, both Nomex and Aluminium?

In particular, are they regular hexagons in shape (all sides the same length) and is the cell size measured from one flat side to the opposing flat side, rather than corder to corner or some other measurement?

Are there any variations in this in the Nomex and Aluminium you stock, or are they all the same?

Thanks for your help.
Reply
jt393
jt393
Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)Supreme Being (158 reputation)
Group: Forum Members
Posts: 4, Visits: 15
Thanks Warren, that is a really helpful response - the extra information especially.

I am interested in the designed geometry for modelling purposes, so completely understand about the tolerances and that it's never going to be absolutely precise.

And the cell size is measured across the cell, as in the dc in the diagram below?
http://www.sensorprod.com/news/white-papers/2003_etfs/image02.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search