Recommended Epoxy for DIY Prepreg


Author
Message
p3carbon
p3carbon
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 2, Visits: 30
I'm about to test some parts made from prepreg material and I'd like to produce our own prepreg similar to the method in David Algie's now famous video. If I understand correctly, I can obtain a b-stage cure with our existing array of epoxies and vinyl ester resins simply by changing the catalyst??? Can anyone using this method of DIY prepreg production recommend a good epoxy and catalyst to use?  
Reply
ChrisR
ChrisR
Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)Supreme Being (3.1K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
The Huntsman resins are great, I used them all the time.

Depending on where you are, you could try mouldlife in the UK, if you're in europe then try searching for Gazechim Group (they've just bought out mouldlife)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search