Pre-Pregs
Recommended Epoxy for DIY Prepreg
http://www.talkcomposites.com/Topic15845.aspx
By p3carbon
-
3/29/2015 2:06:06 AM
I'm about to test some parts made from prepreg material and I'd like to produce our own prepreg similar to the method in David Algie's now famous video. If I understand correctly, I can obtain a b-stage cure with our existing array of epoxies and vinyl ester resins simply by changing the catalyst??? Can anyone using this method of DIY prepreg production recommend a good epoxy and catalyst to use?
By ChrisR
-
4/17/2015 10:34:47 AM
The Huntsman resins are great, I used them all the time.
Depending on where you are, you could try mouldlife in the UK, if you're in europe then try searching for
Gazechim Group (they've just bought out mouldlife)