Hi all,
I am a beginner in composite infusion and before making my first part, I am asking myself some questions :
Could you know a way to make IN2 resin UV stable?
Am I oblige by using a gelcoat or a polish UV stable?
Can you tell me how do the IN2 resin parts live in outside surrondings.

Many thanks
Reply
Olivier44
Olivier44
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 2, Visits: 4
It is what I thought.
Thanks for your advices.
Bye from France
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search