It is what I thought.
Thanks for your advices.
Bye from France
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You would need a UV stable gel coat or to lacquer the part with a UV stable clear coat - preferably a 2k paint.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
As far as I understand, the IN2 resin is quite UV resistant for an epoxy, so it depends how much exposure the part will have. 

If it needs to be UV Proof, so totally UV stable, then it can't be done without a coating of some kind.
Olivier44
Olivier44
Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)Forum Member (34 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Hi all,
I am a beginner in composite infusion and before making my first part, I am asking myself some questions :
Could you know a way to make IN2 resin UV stable?
Am I oblige by using a gelcoat or a polish UV stable?
Can you tell me how do the IN2 resin parts live in outside surrondings.

Many thanks