Which spray nozzle for Pattern Coat Primer?


Author
Message
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Hi

My cup gun came with a FN6 nozzle suitable for gelcoats, but which is what is the ideal size for spraying the Pattern Coat and also the High Gloss finish?

Thanks

Mark
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Yes you can spray the Pattern-Coat Primer by cup gun. Use the standard FN6 nozzle and thin down the Primer using 25% of pure acetone. That should thin it to a sprayable consistancy.

For the Pattern-Coat Hi Gloss, application by gelcoat spray gun will yield the best results and mean much less finishing work is required. When spraying, thin the Pattern-Coat™ Hi Gloss using pure acetone at a ratio of 25%.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search